Fibre Glass Resin
Fibre Glass Resin
Author
Discussion

jay jay bee

Original Poster:

156 posts

201 months

Saturday 28th February 2015
quotequote all
Can anyone advise a product/resin mix to re-coat the inside of my front mud guards/rear wheel arches. Thanks in advance.

Edited by jay jay bee on Saturday 28th February 20:07

glenrobbo

39,453 posts

173 months

Saturday 28th February 2015
quotequote all
Alfie Boe is the man to ask.
That was his job at the old Bristol Ave factory.

Sorry I can't be more helpful JJB, it's not my specialist subject.

rev-erend

21,603 posts

307 months

Saturday 28th February 2015
quotequote all
I always use CFS

http://www.cfsnet.co.uk/

Seem reliable.

Products are good.

Alan Whitaker

2,054 posts

205 months

Saturday 28th February 2015
quotequote all
Hi
I use these for my materials, they are North East

http://www.ecfibreglasssupplies.co.uk/


Are you repairing or just adding a finish coat to make look good?

Alan

jay jay bee

Original Poster:

156 posts

201 months

Saturday 28th February 2015
quotequote all
Just a finish coat to improve appearance.

Alan Whitaker

2,054 posts

205 months

Saturday 28th February 2015
quotequote all
Hi
Unless you grind all the muck off, the resin won't stick, you need to use a flap wheel to clean it, why don't you use a good stone chip after cleaning it up.

Alan

Fibre-ron

112 posts

260 months

Sunday 1st March 2015
quotequote all
what you need is called flow coat. its a mix of gelcoat and resin,