Clam Contruction Question
Clam Contruction Question
Author
Discussion

stampede

Original Poster:

266 posts

249 months

Wednesday 27th September 2006
quotequote all
A quick question from the uninitiated.

Are the fibreglass panels of a Lotus constructed in the same way as a boat in that is there a coloured gel coat with a fibre/resin backing or is it a neutral gelcoat that is subsequently painted?

S690

Stonie

140 posts

253 months

Wednesday 27th September 2006
quotequote all
They are a light/mid grey gelcoat from what I've seen, then spray painted whatever colour.

Arno

349 posts

309 months

Thursday 28th September 2006
quotequote all
The S2 uses pretty much no gelcoat at all, as these are not made using the old style method of putting woven glass mats in a shapen and putting resin onto them.

The S2 clams are made using an injection-moulding process using chopped glass stands in an epoxy, which is then injected under high pressure in stainless steel moulds.

This process results in a better resin-glass ratio (less resin), making it lighter, and also does not requie a gelcoat as the moulds used are ploshed smooth, so the resin does not 'stick' to them.

It's a little more difficult to repair because of this low resin content and short glassfibre strands, but traditional fibreglass repair methods do still work.

Bye, Arno.

gooby

9,269 posts

265 months

Thursday 28th September 2006
quotequote all
Arno said:
The S2 uses pretty much no gelcoat at all, as these are not made using the old style method of putting woven glass mats in a shapen and putting resin onto them.

The S2 clams are made using an injection-moulding process using chopped glass stands in an epoxy, which is then injected under high pressure in stainless steel moulds.

This process results in a better resin-glass ratio (less resin), making it lighter, and also does not requie a gelcoat as the moulds used are ploshed smooth, so the resin does not 'stick' to them.

It's a little more difficult to repair because of this low resin content and short glassfibre strands, but traditional fibreglass repair methods do still work.

Bye, Arno.


Wow! Good info - thanks Arno

gooby

9,269 posts

265 months

Thursday 28th September 2006
quotequote all
Aron - is it a multi-point pressure injection? I suppose the sprue's would be easy to conceal, jut but them on the inside!

MiniDiva

1,227 posts

252 months

Thursday 28th September 2006
quotequote all
From what I recall being told at the factory, the S2 Exige clams are still hand laid.

My Exige clam is all scruffy & rough on the inside because of this, compared to the Elise which is nice & smooth.

The old clam that came off the front of mine (after a hare headbutted it), appeared to have an orange layer underneath the orange paint (not primer though) which i always assumed was the gelcoat. The new clam is green underneath the new paint - which doesn't really help with hiding the stone chips like the orange did!!

Arno

349 posts

309 months

Friday 29th September 2006
quotequote all
Yup.. S2 Exige clams are hand-laid, just like S1 clams.

Production volume is too small to warrant the use of the normal S2 production method.

Does make the Exige clams heavier than normal S2 clams though.