Chassis / Suspension Paint post rust removal.
Chassis / Suspension Paint post rust removal.
Author
Discussion

TEKNOPUG

Original Poster:

20,516 posts

236 months

Tuesday 24th November
quotequote all
I have some old struts that I'm going wire wheel and then apply Bilt Hamber Deox rust remover. I then need to paint them. I don't want the expense and hassle of 2 part epoxy solvent primer & top coat (these are strut bodies with Koni inserts and I have some much better condition bodies that I can cut up in future), just a 1 tin water based solution, that should be good for a year or so.

Any personal recommendations? Looking at Rust-Oleum Aqua but can't find a UK supplier or Buzzworld Chassis One etc.
Tuesday 24th November
quotequote all
For a single-tin water-based option, the water-based 'hammerite style' textured rustproof paints from the DIY multiples are the usual go-to and cover straight over treated rust without a separate primer - fine for a year-plus on chassis parts that see no abuse.Two things I'd flag:1) The tannin coating the rust converter leaves behind is actually paint-friendly, but it must be fully dry (a day in a warm garage) before anything water-based goes over it. If it's still damp, the water in the paint re-wets the tannin and you get flash rust under the film within days.2) If the strut bodies are scuffed to bright metal after wire wheeling, a 1K water-based paint needs a proper key to the surface - a wipe-on etching primer before the top coat is the difference between lasting a year and lifting at every stone chip within months. On bare steel alone, single-tin water-based paints fail fast.If you can stretch to a second tin, a proper 2K (activated) water-based system over the converted rust goes several winters without retouch. But if these bodies are genuinely disposable until the next project, the single tin is fine - I've had the same approach on exhaust and subframe brackets get through one salted winter with reasonable results.

Edited by Repulsive_War_018x on Tuesday 24th November 13:09

steveo3002

11,246 posts

205 months

Tuesday 24th November
quotequote all
how much does the tin of water based cost ?

if you are really going to soak until fully derusted , then a aerosol of epoxy is only £20 and would be doing it right and long lasting

if you really dont care grab whatever poundland has on the shelves and crack on

TEKNOPUG

Original Poster:

20,516 posts

236 months

Tuesday 24th November
quotequote all
The 2k epoxies I was looking at originally, all suggest that respiratory filters are mandatory for indoor use, which increases the cost considerably. Hence why I was looking at water based products.

_Rodders_

5,520 posts

50 months

Tuesday 24th November
quotequote all
But then how would you smell that lovely smell hehe

POR15 is pretty good from experience.

steveo3002

11,246 posts

205 months

Tuesday 24th November
quotequote all
TEKNOPUG said:
The 2k epoxies I was looking at originally, all suggest that respiratory filters are mandatory for indoor use, which increases the cost considerably. Hence why I was looking at water based products.
theyre non isocyanate if thats worrying you ,,,but yeah wise to use a mask still

TEKNOPUG

Original Poster:

20,516 posts

236 months

Tuesday 24th November
quotequote all
Ok, lots of good suggestions. I think I see how much rust I can remove from a strut and what condition the metal is in afterwards, then decide whether it's worth spending money to preserve them or not

Belle427

12,069 posts

264 months

Tuesday 24th November
quotequote all
Rustoleum combi colour will do, much better than hammerite and can be kept for other things if you buy a colour like black.

DaveF-SkinnysAutos

233 posts

15 months

Tuesday 24th November
quotequote all
Without question 2K epoxy is the best by a long way, you can get it in aerosols, you pull the pin to activate the hardener, it single use and you bin what you don't use.You then have a completely waterproof surface that is etched to the metal better than any other product.

You should wear a mask, the Gerson 8000 are good for DIY use in ventilated areas as an occasional use, they protect from 2K for a decent number of hours. They are all over Ebay and Amazon etc for under £30.

The alternate that I use on bare metal is obviously remove as much rust as possible by mechanical means, ie, wire wheel, sanding etc, then the Bilt Hamber detox gel, then I use Miparox emulsion, not the aerosol, the brush on emulsion, it works as both a rust converter and a primer for whatever you want to put on after, as its brushed on its not the cleanest finish but for chassis parts its excellent. It converts and seals any rust underneath and leaves a sold surface for whatever you then want to use as a finishing coat.

If you are happy you have removed every speck of rust and don't need a rust converter (brave shout!) then you can go with any DTM (direct to metal), any paint supplier will sell it you half the price of hammerite and it will do the job for a year.