Aston Martin Bodywork Corrosion Claim
Aston Martin Bodywork Corrosion Claim
Author
Discussion

R8VBV

Original Poster:

348 posts

145 months

Tuesday 24th February 2015
quotequote all
The initial message was deleted from this topic on 23 March 2015 at 13:41

DAVIDOXE

495 posts

144 months

Tuesday 24th February 2015
quotequote all
Did you buy it from a main dealer?

mjk1

233 posts

256 months

Tuesday 24th February 2015
quotequote all
Has this panel been re sprayed? This isn't the usual area for the paint bubbling problem commonly seen.

simonpa

381 posts

313 months

Tuesday 24th February 2015
quotequote all
R8VBV said:
The garage I bought the car from, sold it new and looked after it it's entire life, before I bought it. They said it's had no work and the HPI was clear.

It is strange, but from what I understand, it only take a person to touch the bare metal without gloves and the oxidization can happen years later.
Lol - which dealer was this?

It's a very unusual place for this to happen - looks more like a failed repair.
It would be interesting to get it checked out by someone who has one of those devices to measure the paint thickness - that would tell you if there was filler underneath...


DAVIDOXE

495 posts

144 months

Tuesday 24th February 2015
quotequote all
I had this on my V8 and the dealer just sorted it.

BigMig

205 posts

141 months

Tuesday 24th February 2015
quotequote all
A magnet will tell you if there's filler in that area, yes I know aluminium is non magnetic, but that part of the structure is actually steel.