Anyone have any experience of the Hi-temp exhaust manifold paints that dont need baking.. i.e. they cure during use?

Are they good value or too good to be true..?!

cheers

clive f

7,259 posts

263 months

Wednesday 10th October 2007
quotequote all
I tried speerex a couple of years ago on my S2, supposed to withstand very high temperatues and advertised as exhaust manifold paint, but it soon comes off, needs regular coating every couple of months or so, waste of time in my opinion .

blitzracing

6,422 posts

250 months

Thursday 11th October 2007
quotequote all
Demon tweeks do a product called Cermakrome, its a very high temperature ceramic piant that needs baking on after shot blasting the surface first. I know its used inside and outside exhausts and can be polished to a sheen to help the exhaust flow (on the inside). There are companies out there that will do the tricky business of applying it at a price. Much better than a paint if you can afford it. At the other end of the scale Hammertite (read Halfords)do a high temperature matt black for around £6, you can slap on with a brush. Ive had it on a cast manifold over the summer with no flaking so far, but I suspect it goes thin after a time and needs reapplying.

adam_rbts

Original Poster:

71 posts

237 months

Thursday 11th October 2007
quotequote all
Cheers for the replies.. kinda what I'd figured..

Yeah it was seeing the manifold coatings in Demon tweeks that got me wondering..

Might look into the ceramic paint a bit further..


chrispitman

742 posts

284 months

Thursday 11th October 2007
quotequote all
Had mine done with croma coat but via Tim @ ACT Performance he uses this company http://www.camcoat.u-net.com.

I have the manifolds decatted and coned, then chroma coated outside and black cermic inside. The Y picece is just chroma coat outside.

Coating seem hard, dropped the odd spanner and not make any marks.

realy needs to be done by someone with a industrial oven as the baking temps are extremly high. (I asked around at the time with local powder coaters but there ovens don't get hot enough)

Have some photos if you want.