Surface finish on new MC1 Cam
Discussion
I've just bought an MC1 cam from V8 Developments and my first impression is that the surface finish of the cam lobes is far rougher than I had expected, but then I'm not an expert on cams.
Having spoken to Rob at V8Dev he was a little vague over what sort of surface finish was acceptable. I accept that the cam is probably ground and then case hardened which is likely to affect surface finish, but there is a definite 'visible to the eye' grain structure.
I don't want to spend a lot of time and cost in fitting this for it to need changing again in a few weeks/months does anyone have a more experienced view on this.
[pic]F:\Documents and Settings\All Users\My Documents\My Pictures\MC1 Cam.jpg[/pic]
Mike
Having spoken to Rob at V8Dev he was a little vague over what sort of surface finish was acceptable. I accept that the cam is probably ground and then case hardened which is likely to affect surface finish, but there is a definite 'visible to the eye' grain structure.
I don't want to spend a lot of time and cost in fitting this for it to need changing again in a few weeks/months does anyone have a more experienced view on this.
[pic]F:\Documents and Settings\All Users\My Documents\My Pictures\MC1 Cam.jpg[/pic]
Mike