Can anyone advise a product/resin mix to re-coat the inside of my front mud guards/rear wheel arches. Thanks in advance.

Edited by jay jay bee on Saturday 28th February 20:07

glenrobbo

35,290 posts

151 months

Saturday 28th February 2015
quotequote all
Alfie Boe is the man to ask.
That was his job at the old Bristol Ave factory.

Sorry I can't be more helpful JJB, it's not my specialist subject.

rev-erend

21,421 posts

285 months

Saturday 28th February 2015
quotequote all
I always use CFS

http://www.cfsnet.co.uk/

Seem reliable.

Products are good.

Alan Whitaker

2,054 posts

183 months

Saturday 28th February 2015
quotequote all
Hi
I use these for my materials, they are North East

http://www.ecfibreglasssupplies.co.uk/


Are you repairing or just adding a finish coat to make look good?

Alan

jay jay bee

Original Poster:

143 posts

179 months

Saturday 28th February 2015
quotequote all
Just a finish coat to improve appearance.

Alan Whitaker

2,054 posts

183 months

Saturday 28th February 2015
quotequote all
Hi
Unless you grind all the muck off, the resin won't stick, you need to use a flap wheel to clean it, why don't you use a good stone chip after cleaning it up.

Alan

Fibre-ron

112 posts

238 months

Sunday 1st March 2015
quotequote all
what you need is called flow coat. its a mix of gelcoat and resin,